Knife Steel Chart
Each steel links to its own page. Composition and hardness are shown only when we can point to a source for the number, so some cells are empty for now.
| Steel | Also called | Family | Origin | Carbon | Chromium | Hardness |
|---|---|---|---|---|---|---|
| 10Cr15CoMoV | 10Cr15CoMoV steel | Stainless | China | pending | pending | 58–62 HRC across knife makers' own figures (Xinzuo 60+1 and 60±2, SRM Knives 58–60) |
| 12C27 | Sandvik 12C27, Alleima 12C27 | Stainless | Sweden | 0.6% | 13.5% | 54–61 HRC (the range the producer gives) |
| 14C28N | Sandvik 14C28N, Alleima 14C28N | Stainless | Sweden | 0.62% | 14% | 55–62 HRC (the range the producer recommends) |
| 420HC | 420 High Carbon, 420 HC, ATI 420HC | Stainless | Not tied to one country | 0.40–0.45% | 12.5–13.5% | 56–59 HRC (ATI's hardening response for 420HC); Buck Knives states Rc 58 for its standard steel; Leatherman states 56–58 HRC |
| 440C | AISI 440C, UNS S44004, EN 1.4125 | Stainless | United States | 0.95–1.20% | 16.00–18.00% | About 60 HRC at full hardness (Carpenter Technology's figure); 56–60 HRC across the tempering range in its datasheet |
| 7Cr17MoV | 7Cr17, 68Cr17 | Stainless | China | pending | pending | 56–58 HRC (Xinzuo's figure); 57.2 HRC measured on one plate in a 2023 study |
| 9Cr18MoV | 90Cr18MoV, S46990, S44099 | Stainless | China | 0.85–0.95% | 17.00–19.00% | 56–60 HRC across knife makers' own figures (CIVIVI 58–60, Shan Zu 57–59, Xinzuo 56–60, Boker 56–58) |
| Aogami #2 | Blue Steel #2, Blue Paper #2 | Carbon | Japan | pending | pending | source pending |
| AUS-10 | AUS10 | Stainless | Japan | 0.95–1.10% | 13.00–14.50% | About 60 HRC (the reference value the Aichi group's rolling company gives after a 1050°C quench and 180°C temper) |
| AUS-8 | AUS8, AUS-8A | Stainless | Japan | 0.70–0.80% | 13.00–14.50% | About 59 HRC (the reference value the Aichi group's rolling company gives after a 1050°C quench and 180°C temper) |
| MagnaCut | CPM MagnaCut | Powder stainless | United States | pending | pending | source pending |
| N690 | BÖHLER N690, Bohler N690, N690Co, 1.4528, X105CrCoMo18-2 | Stainless | Austria | 1.08% | 17.3% | Up to 59–61 HRC (the producer's figure, hardened from 1030°C) |
| SG2 | R2, Super Gold 2 | Powder stainless | Japan | pending | pending | source pending |
| Shirogami #2 | White Steel #2, White Paper #2 | Carbon | Japan | pending | pending | source pending |
| VG-10 | VG10, V Gold 10 | Stainless | Japan | pending | pending | source pending |
| X50CrMoV15 | 1.4116, EN 1.4116, 4116, X50 Cr MoV 15 | Stainless | Europe (EN standard grade 1.4116) | 0.50% | 14.50% | About 56 HRC (SIJ Metal Ravne's figure); Böker states 55–56 HRC for its knives in this steel |
Explainers
-
Rockwell Hardness (HRC) Explained for Knife Buyers
What the HRC number on a knife means, how the Rockwell C test works, the ranges steel producers publish, and why harder is not automatically better.
Explainer Draft
Spec & source review We have not handled the products mentioned. Details come from the makers' specifications and the sources listed below. What our evidence labels mean.